Define substantial corrosion, pitting corrosion, edge corrosion, groove corrosion and stress corrosion?
Updated · AI-generated answer
Short answer
- Substantial corrosion: wastage in excess of 75% of allowable margins, but within acceptable limits; for CSR ships: gauged thickness between tnet + 0.5 mm and tnet
- Pitting corrosion: scattered spots/areas with local material reductions greater than surrounding general corrosion
- Edge corrosion: local corrosion at free edges of plates, stiffeners, primary support members and around openings
- Groove corrosion: local corrosion in the form of grooves or channels
- Stress corrosion: cracking caused by the combined action of tensile stress and a corrosive environment
- Mechanism: electrochemical cell in electrolyte (seawater) with anodic metal dissolution
- Primary source: IACS UR Z102 §1.2.17–1.2.20 and IMO A.1049(27) Annex
| Corrosion type | Definition | Location/Appearance |
|---|---|---|
| Substantial | Wastage >75% of allowable margins (CSR: tnet+0.5 mm to tnet) | General structural wastage |
| Pitting | Scattered spots with deeper local attack than surrounding area | Random local pits |
| Edge | Local attack at free edges of plates, stiffeners, around openings | Plate edges, cutouts |
| Groove | Local attack forming grooves or channels | Along weld toes, seams |
| Stress | Cracking from tensile stress + corrosive environment | High-stress areas, welds |
How this answer is built
The rules and references the full answer draws on, from international rules down to practice on board.
The full answer draws on4 sources in 3 groups
- International rules (IMO)Conventions, codes, resolutions and circulars
- A.1049(27) Annex Annex APart A §1.2.9
- MSC.461(101) Annex A§8.2 · §8.3
- Class society (IACS)Unified requirements, interpretations and recommendations
- IACS UR Z10.2§1.2.17 · §1.2.18
- Engineering practiceHow it is done on board
- Corrosion & Protection
Full answer
The full answer explains each point step by step, with the regulations and figures behind it and the discussion from other candidates. It is in the MEO Class I section of the Marine One forum, open to members enrolled for the MEO Class I exam.