MEO Class I · Oral · asked at MMD Chennai

Have you done drydock? How do you select steel and what grades are used?

Updated · AI-generated answer

Short answer

  • Location threshold: 0.3 m below lower ice waterline
  • Submerged plating: IACS UR S6 Tables 6 and 7 for minimum grade
  • Weather-exposed plating: IACS UR I2 Table 8 for minimum grade
  • Equivalency check: IACS Rec 47 §4.2.3 (chemical composition, mechanical properties, heat treatment, tolerances)
  • Normal strength grades: A, B, D, E
  • Higher strength grades: AH, DH, EH
  • Low temperature grades: F32, F36, F40
  • Welding compliance: UR W17 and UR W28

How this answer is built

The rules and references the full answer draws on, from international rules down to practice on board.

The full answer draws on4 sources in 2 groups
  1. Class society (IACS)Unified requirements, interpretations and recommendations
    • IACS UR I2§I2.12.3 · §I2.12.4
    • IACS Recommendation 47§4.2.3
    • IACS UR S6Use of Steel Grades for Various Hull Members
  2. Engineering practiceHow it is done on board
    • Drydocking

Full answer

The full answer explains each point step by step, with the regulations and figures behind it and the discussion from other candidates. It is in the MEO Class I section of the Marine One forum, open to members enrolled for the MEO Class I exam.