What it requires
A hull painting scheme is the planned set of coatings on a ship's outer hull. Below the waterline it has two jobs. It stops corrosion of the steel, and it stops marine growth (fouling) from building up. A smooth, clean hull needs less power, so the scheme also affects fuel use.
What the rules require
- Anti-fouling controls. The AFS Convention defines an anti-fouling system as a coating, paint, surface treatment, surface or device used on a ship to control or prevent attachment of unwanted organisms.
- Ships must not apply or re-apply anti-fouling systems that use organotin compounds as biocides (from 1 January 2003).
- From 1 January 2008, ships must either carry no such compounds on their hulls or external surfaces, or carry a barrier coat that stops them leaching from the old coating underneath.
- By amendment in resolution MEPC.331(76), ships must not apply or re-apply anti-fouling systems containing cybutryne from 1 January 2023.
- A ship that already had cybutryne in the outer coat on 1 January 2023 must remove it, or seal it with a barrier coat. This is due at the next scheduled renewal of the anti-fouling system after that date, and no later than 60 months after the cybutryne coating was last applied. Some ships are excepted, such as ships not on international voyages.
- Survey and certificate. Ships of 400 gross tonnage and above on international voyages need an initial survey, and a further survey whenever the anti-fouling system is changed or replaced. They carry an International Anti-fouling System Certificate, supplemented by a Record of Anti-fouling Systems. The certificate ceases to be valid if the system is changed or replaced and the certificate is not endorsed.
- Smaller ships. Ships of 24 metres or more in length but under 400 gross tonnage, on international voyages, carry a Declaration on Anti-fouling System signed by the owner or agent. It is backed by documents such as a paint receipt or contractor invoice.
- Waste. Each Party must make sure that waste from applying or removing a controlled anti-fouling system is collected and disposed of safely.
- Hull markings. The load line marks must be painted white or yellow on a dark ground, or black on a light ground, and also be permanently marked. The IMO (International Maritime Organization) number must be permanently marked in a contrasting colour, at least 200 mm high on the hull or superstructure.
What IMO guidance recommends
- The 2023 Biofouling Guidelines, resolution MEPC.378(80), recommend an anti-fouling system on all submerged surfaces where fouling may attach. They replaced the 2011 guidelines, MEPC.207(62).
- Choose the coating for the ship's speed, trading pattern, idle periods, water temperature and salinity, the cleaning methods available, and the docking cycle.
- The coating's life should be longer than the interval between dry-dockings.
- Apply, repair and re-apply the coating to the maker's guidance, including surface preparation.
- Give niche areas special care: sea chests and gratings, thruster tunnels, rudder hinges, stern tube seals, anodes and pitot housings. Edges, corners and welds should be smooth and given adequate film thickness.
- Propellers are usually polished rather than coated. A foul-release or other coating may be used where suitable.
- Move docking block positions at each docking, or make other arrangements, so that areas under the blocks get anti-fouling at least at alternate dockings.
- Keep a ship-specific Biofouling Management Plan and a Biofouling Record Book. The record book is kept for the life of the ship and records coating repairs, including the percentage of hull recoated.
- Inspect in water within 12 months of applying the coating if the ship does not monitor performance. If monitoring shows good performance, the first inspection may be up to 18 months after. Later inspections are at least every 12 to 18 months.
- The SEEMP guidelines, resolution MEPC.346(78), add that docking intervals should be tied to performance monitoring. They note that a smoother hull generally means better fuel efficiency. Full removal and replacement of the underwater paint may avoid the roughness that builds up from repeated spot blasting over many dockings.
What shipyards and makers do in practice
- The scheme is written by the paint maker and agreed with the owner before docking. It states, for each hull area, the surface preparation, the products, the number of coats and the film thickness for each coat.
- A typical underwater scheme has anti-corrosive coats on the steel, a tie coat where the maker calls for one, and then the anti-fouling or foul-release top coats. The boot-top and topsides get their own anti-corrosive and finish coats.
- The maker's technical data sheet sets the limits for surface preparation, humidity, steel temperature, overcoat times and the time before undocking. The yard and the paint inspector check them on each coat.
- Common types are self-polishing anti-fouling, which wears away slowly and releases biocide, and biocide-free foul-release coatings, which give a slippery surface that growth cannot grip well.
- Damaged areas are spot-blasted and touched up. Where breakdown is widespread, the yard blasts and recoats the whole area.
Related rule for tanks (not the outer hull)
- SOLAS (Safety of Life at Sea) regulation II-1/3-2 requires dedicated seawater ballast tanks, and double-side skin spaces of bulk carriers of 150 m in length and upwards, to be coated during construction to the performance standard for protective coatings, resolution MSC.215(82). Coating maintenance must be in the ship's maintenance scheme.
- That standard targets a useful coating life of 15 years. It calls for blasting to Sa 2½ with a profile between 30 and 75 µm, and a nominal dry film thickness of 320 µm with the 90/10 rule for epoxy-based systems. It bans blasting and painting when the relative humidity is above 85% or the steel is less than 3°C above the dew point. These figures apply to ballast tanks, not to the outer hull.
Why it is asked
Hull condition is one of the main external causes of high fuel consumption. Docking is also when the Chief Engineer must check the yard's paint work before the ship refloats. Examiners therefore ask about the painting scheme in fuel-consumption and dry-dock questions.
Typical questions are:
- What are the methods to reduce hull friction?
- What checks do you make as Chief Engineer before undocking?
- The ship has just come out of dry dock and fuel consumption has risen. Write the email to the superintendent: inspections, findings and suggested repairs.
- What preparation, coordination and division of duties do you plan for entering dry dock, and what do you check with the yard before coming out?
- How do hull condition, weather, the fuel system and propeller damage affect fuel consumption, and how can they be controlled?
The examiner looks for the link between hull roughness, fouling and fuel use. They also look for knowledge of the AFS Convention and its certificate, and of practical checks such as coating inspection, areas under the blocks, sea chests and anodes.
Regulations and key figures
| Instrument | Locus | What it requires |
|---|---|---|
| AFS Convention 2001 | Article 2(2) | Defines an anti-fouling system as a coating, paint, surface treatment, surface or device used to control or prevent attachment of unwanted organisms |
| AFS Convention 2001 | Annex 1 | No application or re-application of organotin biocides (from 1 January 2003); from 1 January 2008, no organotin on the hull or a barrier coat over it |
| MEPC.331(76) | Amendment to AFS Annex 1 | No application or re-application of cybutryne from 1 January 2023; existing cybutryne outer coat removed or sealed at the next renewal, no later than 60 months after last application |
| AFS Convention 2001 | Article 5 | Wastes from applying or removing controlled anti-fouling systems collected and disposed of safely |
| AFS Convention 2001 | Annex 4, regulation 1 | Ships of 400 GT and above on international voyages: initial survey, and survey when the anti-fouling system is changed or replaced |
| AFS Convention 2001 | Annex 4, regulations 2 and 4 | International Anti-fouling System Certificate with a Record of Anti-fouling Systems; certificate invalid if the system is changed without endorsement, or on change of flag |
| AFS Convention 2001 | Annex 4, regulation 5 | Ships of 24 m or more and under 400 GT on international voyages carry a Declaration on Anti-fouling System |
| MEPC.378(80) | Sections 6.3 to 6.12 | Choice, installation and repair of anti-fouling systems; niche areas; coating life longer than the docking interval; docking block positions varied |
| MEPC.378(80) | Sections 8.4 to 8.6 | In-water inspection within 12 months of application without performance monitoring, up to 18 months with good monitoring results, then at least every 12 to 18 months |
| MEPC.378(80) | Section 11 | Biofouling Record Book kept for the life of the ship, recording coating repairs including the percentage of hull recoated |
| MEPC.346(78) | Sections 5.3.10 to 5.3.13 | Docking intervals tied to performance assessment; in-water hull inspection; full replacement of underwater paint to avoid roughness from repeated spot repairs; smoother hull, better fuel efficiency |
| Load Lines Convention 1966 | Annex I, regulation 8 | Load line marks painted white or yellow on dark ground, or black on light ground, and permanently marked |
| SOLAS | Regulation XI-1/3.4 and 3.5 | IMO number permanently marked in a contrasting colour, not less than 200 mm high on the hull or superstructure |
| SOLAS | Regulation II-1/3-2.2 and 3-2.4 | Ballast tanks, and double-side skin spaces of bulk carriers of 150 m and upwards, coated to the performance standard for protective coatings; coating maintenance in the ship's maintenance scheme |
| MSC.215(82), performance standard for protective coatings | Annex, sections 2.8 and 4.1 and table 1 | For ballast tanks: target useful life 15 years; Sa 2½ with 30 to 75 µm profile; nominal dry film thickness 320 µm with the 90/10 rule; no blasting or painting above 85% relative humidity or within 3°C of dew point |
| IACS (International Association of Classification Societies) Recommendation 82 | Glossary | Antifouling is paint for underwater hull areas; defines "good", "fair" and "poor" condition of hard coatings |
| IACS UR Z23 | Table 1 | At new construction, records of anti-fouling application and paint specification kept in the ship construction file |
| Merchant Shipping Act 2025 | Section 134(1)(b) | Every vessel complies with the Anti-Fouling Systems Convention, as applicable |
| Merchant Shipping (Control of Anti-fouling System) Rules, 2016 | Rules 3 to 5 | Indian ships comply with AFS Annex 1; ships of 400 GT and above on international voyages or plying the Indian coast surveyed; International or Indian Anti-Fouling System Certificate issued |
On board
The painting scheme is agreed between the company, the paint maker and the yard. Ship's officers check that it is carried out and recorded.
Chief Engineer (Class 1)
- Agrees the docking work list with the superintendent, including hull preparation and painting.
- Checks the hull before painting: fouling, coating breakdown, pitting, damage under the blocks, and anode wastage.
- Checks that sea chests, gratings, the rudder, thrusters, the stern tube seal area and anodes are cleaned and coated as the scheme requires.
- Before undocking, inspects the finished paint and confirms that the areas under the blocks have been dealt with. Confirms that anodes and sea chest gratings are refitted and that drain plugs are closed.
- Confirms that the AFS certificate or its record is endorsed when the anti-fouling system is changed, and that the Biofouling Record Book is updated.
- After docking, compares fuel consumption and speed with the period before. Reports a rise to the superintendent with possible causes: paint failure, early fouling, propeller roughness or damage.
Second Engineer (Class 2)
- Supervises sea chest cleaning and coating, and the work on grating, valves and anodes.
- Keeps the docking records and photographs of hull and sea chest condition.
- Checks the paint maker's records of coats applied where the Chief Engineer delegates this.
Engineer Officer of the Watch (Class 4)
- Records speed, revolutions and fuel consumption accurately at sea. These figures show the hull's performance between dockings.
- Reports signs of fouling in sea chests and coolers, such as rising sea water temperatures.
Electro-Technical Officer (ETO)
- Maintains the impressed current cathodic protection system, where fitted, and records its readings. Checks its anodes and reference cells during docking.
- Maintains any marine growth prevention system for sea chests and cooling water.
India. The Merchant Shipping Act 2025 requires every vessel to comply with the Anti-Fouling Systems Convention (section 134). The Merchant Shipping (Control of Anti-fouling System) Rules, 2016, made under the 1958 Act, continue in force under the savings clause of section 324 until revoked. They require surveys of ships of 400 gross tonnage and above on international voyages or plying the Indian coast. Such ships carry an International or an Indian Anti-Fouling System Certificate, issued by DGMA or a recognised organisation.
Related topics
- Dry-docking
- Hull cleaning and blasting
- Hull survey in dry dock
- Docking plan and block preparation
- Sacrificial anode renewal
- Sea chest and shipside valve overhaul
- Propeller removal and polishing
- Undocking and refloating
- MARPOL (the convention on pollution from ships) Annex VI, regulation 26: Ship Energy Efficiency Management Plan
Traps and follow-ups
- Using ballast tank figures for the hull. The figures of MSC.215(82) (320 µm, Sa 2½, 85% humidity, 3°C above dew point) are set for ballast tanks. For the outer hull the paint maker's specification governs.
- Forgetting the barrier coat. A ship carrying an old organotin or cybutryne coat may seal it with a barrier coat instead of removing it.
- Not endorsing the certificate. If the anti-fouling system is changed and the certificate is not endorsed, the certificate is no longer valid.
- Forgetting the areas under the blocks. These areas get no paint unless block positions are moved or other arrangements are made.
- Polishing versus painting the propeller. Propellers are normally polished. A rough propeller raises fuel use just as a fouled hull does.
- Blaming the paint too early. A rise in fuel use after docking can also come from propeller damage, weather or fuel system faults. The report should rule these out.
Likely follow-ups:
- What is the difference between self-polishing and foul-release coatings?
- What do "good", "fair" and "poor" coating condition mean?
- How does cathodic protection work alongside the paint scheme?
- Which ships need an International Anti-fouling System Certificate, and which need a Declaration?
- What would you record in the Biofouling Record Book after docking?